StormGlass Meets or Exceeds the Following Standards |
UL 972
|
Burglary-Resistant Glazing
|
ASTM F1233 Class 1
|
Standard Test Method for Security Glazing
|
CPSC 16CFR 1201 Cat II
|
Safety Glazing
|
ANSI Z 97.1
|
Safety Glazing
|
ASTM E1886
|
Impact and Cyclic Pressures
|
Miami Dade Protocols
|
PA 201, PA 202, PA 203
|
Miami Dade NOA # 03-0514.15
|
Expires December 11, 2008
|
Product Configuration |
Outboard Lite
|
Interlayer
|
Inboard Lite
|
Minimum Thickness
|
Average Thickness
|
Maximum Thickness
|
Weight lbs/sq ft
|
| 1/8" (3mm) |
0.075" (1.90mm) |
1/8" (3mm) |
.301 |
.325 |
.347 |
3.8 |
| 3/16" (5mm) |
0.075" (1.90mm) |
3/16" (5mm) |
.431 |
.445 |
.477 |
5.3 |
| 1/4" (6mm) |
0.075" (1.90mm) |
1/4" (6mm) |
.509 |
.521 |
.567 |
6.8 |
*Notes: For hurricane-resistant glazing applications StormGlass should be used as a component in a tested system.
The actual glass thickness and the maximum size is determined by this system testing. When insulating glass is